SAE AMS5225
Iron-Nickel Alloy, Strip, 49Fe - 5.3Cr - 42Ni - 2.5Ti - 0.55Al, Solution Heat Treated, Cold Rolled, 50% Reduction.
This specification covers an iron-nickel alloy in the form of strip.This strip has been used typically for diaphragms, leaf springs, and helical springs, requiring a precipitation-hardenable alloy with a temperature coefficient of modulus of elasticity of -20 to +20 x 10-6 per degree Fahrenheit from -50 to +150 °F (-36 to +36 x 10-6 per degree Celsius from -46 to +66 °C) after suitable heat treatment, but usage is not limited to such applications.
History:Standard | Published | Revision | Status |
---|---|---|---|
AMS5225F | 2009-04-14 | Latest | |
AMS5225E | 2000-05-04 | Historical | |
AMS5225D | 1994-04-01 | Historical | |
AMS5225C | 1982-04-01 | Historical | |
AMS5225B | 1974-12-01 | Historical | |
AMS5225A | 1963-07-01 | Historical | |
AMS5225 | 1955-08-01 | Historical |