SAE AMS4147D
Aluminum Alloy Forgings, 5.6Zn - 2.5Mg - 1.6Cu - 0.23Cr (7075-T7352) Solution Heat Treated, Stress Relieved by Compression, and Overaged.
This specification covers an aluminum alloy in the form of die and hand forgings.
History:Standard | Published | Revision | Status |
---|---|---|---|
AMS4147D | 2007-02-27 | Latest | |
AMS4147C | 1992-07-01 | Historical | |
AMS4147B | 1985-04-01 | Historical | |
AMS4147A | 1978-04-01 | Historical | |
AMS4147 | 1968-05-01 | Historical |