SAE AMS2412G
Plating, Silver Copper Strike, Low Bake.
This specification covers the engineering requirements for silver deposited on metal parts with a copper strike between the basis metal and the silver deposit.
This process has been used typically to provide a bearing surface and to prevent galling or seizing of metal surfaces of parts made of materials where a high baking temperature may be detrimental to the properties of the basic material.