SAE AS7482A

Studs, Corrosion and Heat Resistant Steel, UNS S66286 Tensile Strength 130 ksi 1800 °F Solution Heat Treated, Aged Before Roll Threading Procurement Specification.

More details

Download

PDF AVAILABLE FORMATS IMMEDIATE DOWNLOAD
$29.92 tax incl.

$68.00 tax incl.

(price reduced by 56 %)

1000 items in stock

Standard:
  • AS7482
  • Revision: A
Reaffirmed:
  • 2006-05-08
Revised:
  • 1996-10-01
Revision:
  • Historical. Access the latest revision: AS7482B
Issuing:
  • E-25 General Standards For Aerospace And Propulsion Systems
Scope:

This specification covers studs made from a corrosion and heat resistant, age hardenable iron base alloy of the type identified under the Unified Numbering System as UNS S66286. the following specification designations and their properties are covered:AS7482 130 ksi minimum ultimate tensile strength at room temperature 70 ksi stress-rupture strength at 1200 °FAS 7482-1 130 ksi minimum ultimate tensile strength at room temperature78 ksi minimum ultimate shear strength at room temperatureAS7482-2 130 ksi minimum ultimate tensile strength at room temperature

History:
StandardPublishedRevisionStatus
AS7482B2009-09-01LatestRevised
AS7482A1996-10-01HistoricalReaffirmed
AS74821995-05-01HistoricalReaffirmed
AKA:
  • SAE AS 7482
Sector:
  • Aerospace
Topic:
  • Parts

Contact us