SAE AMS5382H
Cobalt Alloy, Corrosion and Heat Resistant, Investment Castings, 54co 25.5cr 10.5ni 7.5w, as Cast.
This specification covers a corrosion and heat resistant cobalt alloy in the form of investment castings. These castings have been used typically for parts requiring high strength up to 1500 degrees F (816 degrees C) and oxidation resistance up to 2000 degrees F (1093 degrees C), but usage is not limited to such applications. Exposure to elevated temperatures greater than 1200 degrees F (649 degrees C) may result in hardness as high as 44 HRC.
History:Standard | Published | Revision | Status |
---|---|---|---|
AMS5382J | 2006-09-08 | Latest | |
AMS5382H | 1993-04-01 | Historical | |
AMS5382G | 1982-01-01 | Historical | |
AMS5382F | 1978-07-01 | Historical | |
AMS5382E | 1969-05-01 | Historical | |
AMS5382D | 1965-09-01 | Historical | |
AMS5382C | 1964-06-01 | Historical | |
AMS5382B | 1952-06-01 | Historical | |
AMS5382A | 1948-09-01 | Historical | |
AMS5382 | 1947-12-01 | Historical |