SAE AMS5853A
Steel, Corrosion and Heat Resistant, Bars and Wire 15Cr 25.5Ni 1.2Mo 2.1Ti 0.006B 0.30V, Consumable Electrode Melted 1800°F (982°C) Solution Treated and Work-Strengthened 160 ksi (1103 MPa) Tensile Strength.
This specification covers a corrosion and heat resistant steel in the form of work-strengthened bars and wire 1-1/4 inches (31.8 mm) and under in nominal diameter or least distance between parallel sides.
These bars and wire have been used typically for parts, such as fasteners, requiring room- temperature minimum tensile strength of 160 ksi (1103 MPa) after precipitation heat treatment for use up to 1000 degrees F (538 degrees C) and having oxidation resistance up to 1200 degrees F (649 degrees C), but usage is not limited to such applications.
History:Standard | Published | Revision | Status |
---|---|---|---|
AMS5853C | 2006-06-21 | Latest | |
AMS5853B | 2000-10-01 | Historical | |
AMS5853A | 1993-01-01 | Historical | |
AMS5853 | 1991-10-01 | Historical |