SAE AMS4311A
Aluminum Alloy, Rolled or Forged Rings, 5.6Zn - 2.5Mg - 1.6Cu - 0.23Cr (7075-T7351, 7075-T7352), Solution Heat Treated, Mechanically Stress Relieved, and Precipitation Heat Treated.
This specification covers an aluminum alloy in the form of rolled or forged rings.
History:Standard | Published | Revision | Status |
---|---|---|---|
AMS4311E | 2007-08-24 | Latest | |
AMS4311D | 2003-08-05 | Historical | |
AMS4311C | 1994-07-01 | Historical | |
AMS4311B | 1988-10-01 | Historical | |
AMS4311A | 1983-01-01 | Historical | |
AMS4311 | 1976-07-01 | Historical |